ABSTRACT

In this work, a compound waste material was made up of raw construction waste concrete, waste tiles, and waste bricks was mixed at a weight ratio of 6:3:1. They were ground into recycled fine aggregates (RFA). RFA substituted the local river sand in proportions of 0%, 30%, 50%, 70%, and 100% for preparing recycled fine aggregate concrete (RFAC) with varied water-to-cement ratios. It intended to explore concrete’s mechanical properties and ultrasonic pulse velocity changes before and after high temperatures (300–800°C). The loss on ignition (LOI) of concrete was simultaneously determined to compare the performance in resisting elevated temperature. Test results presented that the higher the replacement ratio of RFA, the gradually higher the reduction in the concrete splitting tensile, compressive, and residual compressive strengths and ultrasonic pulse velocity after elevated temperature exposure. A rapid reduction was especially found at the heated temperature of exceeding 440°C. Furthermore, the old cement paste adhered to the surface of the raw construction waste had a relatively higher LOI. This led to the consequence that the RFAC had an increased LOI with the increment of the RFA replacement ratio, while the LOI of RFAC dropped with the increment of the originally heated temperature.

CO EDITOR-IN-CHIEF:

ASSOCIATE EDITOR:

Nomenclature

ASTM=

American Society for Testing and Materials

CO2=

Carbon dioxide

CaCO3=

Calcium carbonate

CS=

Compressive strength

CH=

Calcium hydroxide

CSH=

Calcium silicate hydrates

Dmax=

Maximum aggregate size

LOI=

Loss on ignition

NAC=

Natural aggregate concrete

NFA=

Natural fine aggregates

NDT=

Nondestructive testing

RA=

Recycled aggregate

RBAC=

Recycled brick aggregate concrete

RC=

Recycled concrete

RCS=

Residual compressive strength

RCAC=

Recycled coarse aggregate concrete

RFA=

Recycled fine aggregates

RFAC=

Recycled fine aggregate concrete

STS=

Splitting tensile strength

w/c=

Water-to-cement ratio

UPV=

Ultrasonic pulse velocity

Disclosure statement

No potential conflict of interest was reported by the author(s).

Additional information

Funding

The author(s) reported that there is no funding associated with the work featured in this article.

Log in via your institution

Log in to Taylor & Francis Online

PDF download + Online access

  • 48 hours access to article PDF & online version
  • Article PDF can be downloaded
  • Article PDF can be printed
USD 61.00 Add to cart

Issue Purchase

  • 30 days online access to complete issue
  • Article PDFs can be downloaded
  • Article PDFs can be printed
USD 199.00 Add to cart

* Local tax will be added as applicable

Related Research

People also read lists articles that other readers of this article have read.

Recommended articles lists articles that we recommend and is powered by our AI driven recommendation engine.

Cited by lists all citing articles based on Crossref citations.
Articles with the Crossref icon will open in a new tab.