1,858
Views
0
CrossRef citations to date
0
Altmetric
Original Articles

Shear bond strength of resin bonded zirconia and lithium disilicate – effect of surface treatment of ceramics and dentin

, , &
Pages 10-19 | Received 07 Dec 2021, Accepted 27 Jan 2022, Published online: 16 Feb 2022

References

  • Larsson C, Wennerberg A. The clinical success of zirconia-based crowns: a systematic review. Int J Prosthodont. 2014;27(1):33–43.
  • Araujo NS, Moda MD, Silva EA, et al. Survival of all-ceramic restorations after a minimum follow-up of five years: a systematic review. Quintessence Int. 2016;47(5):395–405.
  • Quigley NP, Loo DSS, Choy C, et al. Clinical efficacy of methods for bonding to zirconia: a systematic review. J Prosthet Dent. 2021;125(2):231–240.
  • Gardell E, Larsson C, von Steyern PV. Translucent zirconium dioxide and lithium disilicate: a 3-year follow-up of a prospective, practice-based randomized controlled trial on posterior monolithic crowns. Int J Prosthodont. 2021;34(2):163–172.
  • Scaminaci Russo D, Cinelli F, Sarti C, et al. Adhesion to zirconia: a systematic review of current conditioning methods and bonding materials. Dent J (Basel). 2019;7(3):74.
  • Ruyter EI, Vajeeston N, Knarvang T, et al. A novel etching technique for surface treatment of zirconia ceramics to improve adhesion of resin-based luting cements. Acta Biomater Odontol Scand. 2017;3(1):36–46.
  • Oilo M, Haugli K, Ronold HJ, et al. Pre-cementation procedures’ effect on dental zirconias with different yttria content. Dent Mater. 2021;37(9):1425–1436.
  • Sagen MA, Kvam K, Ruyter EI, et al. Debonding mechanism of zirconia and lithium disilicate resin cemented to dentin. Acta Biomater Odontol Scand. 2019;5(1):22–29.
  • Koodaryan R, Hafezeqoran A, Poursoltan S. Effect of dentin surface roughness on the shear bond strength of resin bonded restorations. J Adv Prosthodont. 2016;8(3):224–228.
  • Brigagao VC, Barreto LFD, Goncalves KAS, et al. Effect of interim cement application on bond strength between resin cements and dentin: immediate and delayed dentin sealing. J Prosthet Dent. 2017;117(6):792–798.
  • Ayad MF, Rosenstiel SF, Hassan MM. Surface roughness of dentin after tooth preparation with different rotary instrumentation. J Prosthet Dent. 1996;75(2):122–128.
  • Li YQ, Wang H, Wang YJ, et al. Effect of different grit sizes of diamond rotary instruments for tooth preparation on the retention and adaptation of complete coverage restorations. J Prosthet Dent. 2012;107(2):86–93.
  • Saikaew P, Senawongse P, Chowdhury AA, et al. Effect of smear layer and surface roughness on resin-dentin bond strength of self-etching adhesives. Dent Mater J. 2018;37(6):973–980.
  • Van Meerbeek B, De Munck J, Yoshida Y, et al. Buonocore memorial lecture. Adhesion to enamel and dentin: current status and future challenges. Oper Dent. 2003;28(3):215–235.
  • Frankenberger R, Lohbauer U, Roggendorf MJ, et al. Selective enamel etching reconsidered: better than etch-and-rinse and self-etch? J Adhes Dent. 2008;10(5):339–344.
  • Peutzfeldt A, Sahafi A, Flury S. Bonding of restorative materials to dentin with various luting agents. Oper Dent. 2011;36(3):266–273.
  • Pashley DH, Tay FR, Breschi L, et al. State of the art etch-and-rinse adhesives. Dent Mater. 2011;27(1):1–16.
  • Aker Sagen M, Dahl JE, Matinlinna JP, et al. The influence of the resin-based cement layer on ceramic-dentin bond strength. Eur J Oral Sci. 2021;129(4):e12791.
  • El Mourad AM. Assessment of bonding effectiveness of adhesive materials to tooth structure using bond strength test methods: a review of literature. Open Dent J. 2018;12:664–678.
  • Brown D. BISCO: creating solutions to clinical challenges! Bonding to zirconia, alumina and metal with Z-PRIME Plus. Zirconia; the future of aesthetic indirect restorative dentistry? bisco.com: BISCO. 2010. Available from: https://www.bisco.com/creating-solutions-to-clinical-challenges/
  • Akazawa N, Koizumi H, Nogawa H, et al. Effect of etching with potassium hydrogen difluoride and ammonium hydrogen difluoride on bonding of a tri-n-butylborane initiated resin to zirconia. Dent Mater J. 2019;38(4):540–546.
  • Kuraray N. CLEARFIL CERAMIC PRIMER PLUS Universal prosthetic primer kuraraynoritake.eu: kuraray; 2020. Available from: https://www.kuraraynoritake.eu/en/clearfil-ceramic-primer-plus?gclid=Cj0KCQjwhr2FBhDbARIsACjwLo0t6SEw3YnkGLfHImlumylNvELx4DQDI39GOWQ9TTfBsiBVfqxivbUaAoTGEALw_wcB
  • Vivadent I. Monobond Plus The universal primer ivoclarvivadent.com: ivoclar vivadent. 2020. Available from: https://www.ivoclarvivadent.com/medias/sys_master/celum-connect2-assets/celum-connect2-assets/h74/h69/10384422862878/740499-PRO-Monobond-Plus-PRO-EN-2019.pdf
  • Alavi S, Samie S, Raji SAH. Comparison of lithium disilicate-reinforced glass ceramic surface treatment with hydrofluoric acid, Nd: YAG, and CO2 lasers on shear bond strength of metal brackets. Clin Oral Investig. 2021;25(5):2659–2666.
  • Toman M, Toksavul S. Clinical evaluation of 121 lithium disilicate all-ceramic crowns up to 9 years. Quintessence Int. 2015;46(3):189–197.
  • Kasahara Y, Takamizawa T, Hirokane E, et al. Comparison of different etch-and-rinse adhesive systems based on shear fatigue dentin bond strength and morphological features the interface. Dent Mater. 2021;37(3):e109–e17.
  • Barbon FJ, Moraes RR, Isolan CP, et al. Influence of inorganic filler content of resin luting agents and use of adhesive on the performance of bonded ceramic. J Prosthet Dent. 2019;122(6):566.e1–e11.
  • Standardization IOf. ISO 7711-3:2004 dentistry - diamond rotary instruments - part 3: grit sizes, designation and colour code iso.org: ISO. 2004. Available from: https://www.iso.org/standard/37701.html
  • Abrasives S. Abrasive grade/grit size: santo abrasives AS, fugleveien 4, 1448 Drøbak, Norway. 27th of March 2020. Available from: https://santo-abrasives.com/abrasive-grade-grit-size
  • Vaz RR, Di Hipolito V, D’Alpino PH, et al. Bond strength and interfacial micromorphology of etch-and-Rinse and Self-Adhesive resin cements to dentin. J Prosthodont. 2012;21(2):101–111.
  • Monticelli F, Osorio R, Mazzitelli C, et al. Limited decalcification/diffusion of self-adhesive cements into dentin. J Dent Res. 2008;87(10):974–979.
  • May LG, Kelly JR, Bottino MA, et al. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing. Dent Mater. 2012;28(8):e99–109.
  • Rojpaibool T, Leevailoj C. Fracture resistance of lithium disilicate ceramics bonded to enamel or dentin using different resin cement types and film thicknesses. J Prosthodont. 2017;26(2):141–149.
  • Gerth HU, Dammaschke T, Zuchner H, et al. Chemical analysis and bonding reaction of RelyX unicem and bifix composites-a comparative study. Dent Mater. 2006;22(10):934–941.
  • Cavazos E. Tissue response to fixed partial denture pontic. J Prosthet Dent. 1968;20(2):143–153.
  • Miotti LL, Follak AC, Montagner AF, et al. Is conventional resin cement adhesive performance to dentin better than self-adhesive? A systematic review and Meta-analysis of laboratory studies. Oper Dent. 2020;45(5):484–495.
  • Tribst JPM, dos Santos AFC, da Cruz Santos G, et al. Effect of cement layer thickness on the immediate and long-term bond strength and residual stress between lithium disilicate glass-ceramic and human dentin. Materials. 2021;14(18):5153.
  • Seitz E, Hjortsjö C, Dahl JE, et al. Dentin to dentin adhesion using combinations of resin cements and adhesives from different manufacturers – a novel approach. Biomater Investig Dent. 2020;7(1):96–104.
  • Tani C, Finger WJ. Effect of smear layer thickness on bond strength mediated by three all-in-one self-etching priming adhesives. J Adhes Dent. 2002;4(4):283–289.